Skip to Content
Merck

Quantum dot technology

Quantum Dots

Colloidal quantum dots (QDs) are nanoscale semiconductor crystals with unique optical properties that obey quantum mechanics. They are typically 2-10 nm in diameter and composed of about 10-50 atoms. Generally, due to the quantum size effect, the band gap can be tuned depending on the size of the colloidal nanocrystal, resulting in characteristic emission properties that depend on the grain size, converting the spectrum of incident light into energy of different frequencies. As the grain size decreases, the band gap expands, and the emission wavelength moves toward the shorter wavelength side (Figure 1). Considering its electronic state, it is also known as an artificial atom because its properties are closer to those of an atom than to a bulk material.

Diagram illustrating concepts in nanotechnology and quantum dot physics. Panel A shows energy band diagrams for bulk band structures and quantum dots, highlighting the increased band gap in quantum dots as their size decreases, represented by blue, green, and red circles. Panel B compares two types of quantum dot structures: core type and core/shell type, both centered around a CdSe core with organic ligand molecules attached, and the latter also includes a ZnS shell around the CdSe core.

Figure 1 (A) Quantum dot size vs. energy level. The energy level splitting is due to the quantum size effect; as the nanocrystal size decreases, the semiconductor band gap increases. (B) Structure of CdSe core-type and CdSe/ZnS core/shell-type quantum dots.

Quantum dots not only have tunable emission wavelengths in the visible to infrared regions and narrow spectral half-widths but also exhibit high quantum efficiency while absorbing light at a wide range of wavelengths. Materials can be designed whose chemical, physical, electrical, and optical properties can be tuned by manipulating their energetic state and charge interactions through composition, structure, surface state, crystallinity, and ligands. Their applications range from biological imaging, illumination, and displays to solar cells, security tags, sensors, and quantum information technology, and they are being actively researched and developed for use in a wide variety of applications.1-7,25,30,48

Quantum dots can be fabricated on substrates using lithography, MOCVD, MBE, or other methods of processing in a vacuum environment or vapor phase growth, or colloidal particles by liquid phase synthesis under mild conditions. The former method yields highly crystalline QDs that are precisely controlled and applied to high-performance lasers and integrated circuits. The latter method is relatively easy to synthesize in large quantities and is expected to be used for large-area applications by low-cost printing methods.

The tunable surface chemistry of colloidal quantum dots enables the conjugation of QDs with small molecules, antibodies, and proteins, which, coupled with the excellent optical properties of the QDs, can be used for biosensors, fluorescent labeling, and biological imaging. Surface ligands also play an important role in determining the optoelectronic properties, stability, dispersibility in solvents, functionalization, and charge transport properties of QDs in thin films. Ligand selection during the synthesis process as well as ligand exchange techniques in the liquid and solid phases after synthesis and deposition have been extensively investigated.49,50

Common quantum dots are semiconductors made of cadmium and lead, but the use of these heavy metals is regulated in many applications. Therefore, cadmium-free quantum dots are being developed that retain the same brightness and stability as their conventional counterparts. There is also an active search for synthesis methods that can produce large quantities of laboratory-grade quality at low cost and with good reproducibility. Although the use of quantum dots in markets where small amounts of materials are required for bio-imaging and other applications has been prevalent, their use in displays, lasers, and other electronics fields has begun in earnest with the recent development of high-performance and mass-production technologies.


Typical Quantum Dot Products

Quantum dots are classified into various types according to their composition and structure.

Perovskite Quantum Dots

Five small glass bottles containing Perovskite quantum dots, illuminated under UV light to display a range of colors from blue, green, yellow, orange to red, demonstrating their varying emission wavelengths.

Perovskite quantum dots are a type of direct bandgap semiconductor material characterized by high photoluminescence quantum yield (PLQY) and luminescence intensity and exhibit tunable narrow emission with symmetric emission peaks by changing the composition. It is expected to replace conventional Cd-based quantum dots as a material for displays, X-ray and UV sensors, and light-emitting materials.40 It is also expected to be used as a QD solar cell material, with PCEs exceeding 16% obtained through advanced ligand control technology and device engineering.46,47 Sigma-Aldrich's products are also available in a wide range of applications. Sigma-Aldrich products are characterized by high brightness, narrow FWHM (≤ 20-25 nm), and high PLQY (≥ 60-80%) and are available in organic-inorganic hybrid perovskites (905062) and all-inorganic perovskites represented by CsPbX3 (X = Cl, Br).

Loading

Core-Shell Quantum Dots

The luminescence properties of quantum dots result from the recombination of electron-hole pairs (exciton decay). Exciton decay can also occur without radiation, but the fluorescence quantum yield is reduced. To improve the properties and brightness of semiconductor nanocrystals, there is a method of growing a shell of a different semiconductor material with a larger band gap around it. Shell-coated quantum dots increase the quantum yield by inactivating the radiation-free recombination sites and thus provide high processing properties in a variety of applications. The resulting quantum dots are called core-shell quantum dots and have been widely studied as a means of tuning the photophysical properties of quantum dots.31-33

CuInS2/ZnS Core-Shell Quantum Dots (1 mg/mL in toluene)

CuInS2 is a direct bandgap semiconductor suitable for solar absorption because it does not contain elements such as Cd, Pb, Se, and As and has low environmental and health impact.36,37 CuInS2/ZnS is a quantum dot that exhibits superior quantum efficiency and long-term stability by coating its core with a ZnS shell. It has applications in LED and solar cell development as well as bio-imaging.

Loading

InP/ZnS Core-Shell Quantum Dots (5 mg/mL in toluene)

Oleylamine functionalized
Loading
Oleic acid functionalized
Loading

CdSe/CdS Core-Shell Quantum Rods44,45 (5 mg/mL in hexane)

Loading

CdSe/ZnS ZnS Core-Shell Quantum Dots

Loading

Core-type quantum dots

Core-type quantum dots are single-composition nanocrystals with uniform internal composition. Chalcogenide compounds (selenium compounds or sulfides) of metals such as cadmium and zinc are typical examples. Their photoluminescence and electroluminescence properties can be finely tuned by varying the crystal size.

Graphene quantum dots

Loading

Ag2S, Ag2Se Quantum Dots

Silver chalcogenide quantum dots (Ag2X, X = S, Se, Te) generally have a narrow band gap and near-infrared emission properties.53 They have low cytotoxicity and are attracting attention for applications in bioimaging, nanocarriers, chemical/biosensors, as well as optoelectronics such as infrared sensors and solar cells.54,55

Loading

PbS Core-type quantum dots (oleic acid coated, 10 mg/mL in toluene)

PbS (lead sulfide) quantum dots absorb photons up to the near-infrared region and re-emit them in the near-infrared region. The emission peak is tuned in the range of 900 to 1600 nm by reducing the nanoparticle size to 3 to 7 nm. Their excellent photoabsorption and photoelectric properties make them suitable for near-infrared (NIR) image sensors, infrared LEDs, and infrared photovoltaic cells42 (not only single junction but also in combination with other cells with different absorption wavelengths to build tandem or multi-junction solar cells to improve conversion efficiency).

Emission type
Loading

Absorption type
Loading
1.
Sanderson K. 2009. Quantum dots go large. Nature. 459(7248):760-761. https://doi.org/10.1038/459760a
2.
Graham-Rowe D. 2009. From dots to devices. Nature Photon. 3(6):307-309. https://doi.org/10.1038/nphoton.2009.79
3.
Coe-Sullivan S. 2009. Quantum dot developments. Nature Photon. 3(6):315-316. https://doi.org/10.1038/nphoton.2009.83
4.
Wang X, Ren X, Kahen K, Hahn MA, Rajeswaran M, Maccagnano-Zacher S, Silcox J, Cragg GE, Efros AL, Krauss TD. 2009. Non-blinking semiconductor nanocrystals. Nature. 459(7247):686-689. https://doi.org/10.1038/nature08072
5.
Allen P, Walker B, Bawendi M. 2010. Mechanistic Insights into the Formation of InP Quantum Dots. Angewandte Chemie International Edition. 49(4):760-762. https://doi.org/10.1002/anie.200905632
6.
Li J, Zhao X, Zhao Y, Hu J, Xu M, Gu Z. 2009. Colloidal crystal beads coated with multicolor CdTe quantum dots: microcarriers for optical encoding and fluorescence enhancement. J. Mater. Chem.. 19(36):6492. https://doi.org/10.1039/b908830j
7.
Ang CY, Giam L, Chan ZM, Lin AWH, Gu H, Devlin E, Papaefthymiou GC, Selvan ST, Ying JY. 2009. Facile Synthesis of Fe2O3Nanocrystals without Fe(CO)5Precursor and One-Pot Synthesis of Highly Fluorescent Fe2O3-CdSe Nanocomposites. Adv. Mater.. 21(8):869-873. https://doi.org/10.1002/adma.200801273
8.
Fournier-Bidoz S, Jennings T, Klostranec J, Fung W, Rhee A, Li D, Chan W. 2008. Facile and Rapid One-Step Mass Preparation of Quantum-Dot Barcodes. Angewandte Chemie International Edition. 47(30):5577-5581. https://doi.org/10.1002/anie.200800409
9.
Zhang C, Johnson L. 2007. Microfluidic Control of Fluorescence Resonance Energy Transfer: Breaking the FRET Limit. Angew. Chem. Int. Ed.. 46(19):3482-3485. https://doi.org/10.1002/anie.200604861
10.
Yao H, Zhang Y, Xiao F, Xia Z, Rao J. 2007. Quantum Dot/Bioluminescence Resonance Energy Transfer Based Highly Sensitive Detection of Proteases. Angew. Chem. Int. Ed.. 46(23):4346-4349. https://doi.org/10.1002/anie.200700280
11.
Sun Q, Wang YA, Li LS, Wang D, Zhu T, Xu J, Yang C, Li Y. 2007. Bright, multicoloured light-emitting diodes based on quantum dots. Nature Photon. 1(12):717-722. https://doi.org/10.1038/nphoton.2007.226
12.
Cho K, Lee EK, Joo W, Jang E, Kim T, Lee SJ, Kwon S, Han JY, Kim B, Choi BL, et al. 2009. High-performance crosslinked colloidal quantum-dot light-emitting diodes. Nature Photon. 3(6):341-345. https://doi.org/10.1038/nphoton.2009.92
13.
Rauch T, Böberl M, Tedde SF, Fürst J, Kovalenko MV, Hesser G, Lemmer U, Heiss W, Hayden O. 2009. Near-infrared imaging with quantum-dot-sensitized organic photodiodes. Nature Photon. 3(6):332-336. https://doi.org/10.1038/nphoton.2009.72
14.
Yang J, Dave SR, Gao X. 2008. Quantum Dot Nanobarcodes: Epitaxial Assembly of Nanoparticle?Polymer Complexes in Homogeneous Solution. J. Am. Chem. Soc.. 130(15):5286-5292. https://doi.org/10.1021/ja710934v
15.
Chen D, Viswanatha R, Ong GL, Xie R, Balasubramaninan M, Peng X. 2009. Temperature Dependence of ?Elementary Processes? in Doping Semiconductor Nanocrystals. J. Am. Chem. Soc.. 131(26):9333-9339. https://doi.org/10.1021/ja9018644
16.
Steckel JS, Snee P, Coe-Sullivan S, Zimmer JP, Halpert JE, Anikeeva P, Kim L, Bulovic V, Bawendi MG. 2006. Color-Saturated Green-Emitting QD-LEDs. Angew. Chem. Int. Ed.. 45(35):5796-5799. https://doi.org/10.1002/anie.200600317
17.
Wood V, Panzer MJ, Chen J, Bradley MS, Halpert JE, Bawendi MG, Bulovic? V. 2009. Inkjet-Printed Quantum Dot-Polymer Composites for Full-Color AC-Driven Displays. Adv. Mater.. 21(21):2151-2155. https://doi.org/10.1002/adma.200803256
18.
Leventis HC, O?Mahony F, Akhtar J, Afzaal M, O?Brien P, Haque SA. 2010. Transient Optical Studies of Interfacial Charge Transfer at Nanostructured Metal Oxide/PbS Quantum Dot/Organic Hole Conductor Heterojunctions. J. Am. Chem. Soc.. 132(8):2743-2750. https://doi.org/10.1021/ja909172p
19.
Guo C, Yang H, Sheng Z, Lu Z, Song Q, Li C. Layered Graphene/Quantum Dots for Photovoltaic Devices. Angewandte Chemie International Edition. 49(17):3014-3017. https://doi.org/10.1002/anie.200906291
20.
Lan G, Yang Z, Lin Y, Lin Z, Liao H, Chang H. 2009. A simple strategy for improving the energy conversion of multilayered CdTe quantum dot-sensitized solar cells. J. Mater. Chem.. 19(16):2349. https://doi.org/10.1039/b817000b
21.
Lee Y, Huang B, Chien H. 2008. Highly Efficient CdSe-Sensitized TiO2 Photoelectrode for Quantum-Dot-Sensitized Solar Cell Applications. Chem. Mater.. 20(22):6903-6905. https://doi.org/10.1021/cm802254u
22.
Goodman MD, Xu J, Wang J, Lin Z. 2009. Semiconductor Conjugated Polymer?Quantum Dot Nanocomposites at the Air/Water Interface and Their Photovoltaic Performance. Chem. Mater.. 21(5):934-938. https://doi.org/10.1021/cm803248j
23.
Klem EJD, MacNeil DD, Levina L, Sargent EH. Solution Processed Photovoltaic Devices with 2% Infrared Monochromatic Power Conversion Efficiency: Performance Optimization and Oxide Formation. Adv. Mater.. 20(18):3433-3439. https://doi.org/10.1002/adma.200800326
24.
Tang J, Wang X, Brzozowski L, Barkhouse DAR, Debnath R, Levina L, Sargent EH. 2010. Schottky Quantum Dot Solar Cells Stable in Air under Solar Illumination. Adv. Mater.. 22(12):1398-1402. https://doi.org/10.1002/adma.200903240
25.
Yoffe AD. 2001. Semiconductor quantum dots and related systems: Electronic, optical, luminescence and related properties of low dimensional systems. Advances in Physics. 50(1):1-208. https://doi.org/10.1080/00018730010006608
26.
Nirmal M, Brus L. 1999. Luminescence Photophysics in Semiconductor Nanocrystals. Acc. Chem. Res.. 32(5):407-414. https://doi.org/10.1021/ar9700320
27.
Sargent EH. 2012. Colloidal quantum dot solar cells. Nature Photon. 6(3):133-135. https://doi.org/10.1038/nphoton.2012.33
28.
Zhao Y, Burda C. Development of plasmonic semiconductor nanomaterials with copper chalcogenides for a future with sustainable energy materials. Energy Environ. Sci.. 5(2):5564-5576. https://doi.org/10.1039/c1ee02734d
29.
Medintz IL, Uyeda HT, Goldman ER, Mattoussi H. 2005. Quantum dot bioconjugates for imaging, labelling and sensing. Nature Mater. 4(6):435-446. https://doi.org/10.1038/nmat1390
30.
Vahala KJ. 2003. Optical microcavities. Nature. 424(6950):839-846. https://doi.org/10.1038/nature01939
31.
Bailey RE, Nie S. Core-Shell Semiconductor Nanocrystals for Biological Labeling.405-417. https://doi.org/10.1002/352760247x.ch12
32.
Dorfs D, Eychmüller A. 2006. Multishell Semiconductor Nanocrystals. 220(12):1539-1552. https://doi.org/10.1524/zpch.2006.220.12.1539
33.
Smith AM, Nie S. 2009. Next-generation quantum dots. Nat Biotechnol. 27(8):732-733. https://doi.org/10.1038/nbt0809-732
34.
Vastola G, Zhang Y, Shenoy VB. 2012. Experiments and modeling of alloying in self-assembled quantum dots. Current Opinion in Solid State and Materials Science. 16(2):64-70. https://doi.org/10.1016/j.cossms.2011.10.004
35.
Tan Z, Zhang F, Zhu T, Xu J, Wang AY, Dixon JD, Li L, Zhang Q, Mohney SE, Ruzyllo J. 2007. Bright and Color-Saturated Emission from Blue Light-Emitting Diodes Based on Solution-Processed Colloidal Nanocrystal Quantum Dots. Nano Lett.. 7(12):3803-3807. https://doi.org/10.1021/nl072370s
36.
Coughlan C, Ibáñez M, Dobrozhan O, Singh A, Cabot A, Ryan KM. 2017. Compound Copper Chalcogenide Nanocrystals. Chem. Rev.. 117(9):5865-6109. https://doi.org/10.1021/acs.chemrev.6b00376
37.
Xie R, Rutherford M, Peng X. 2009. Formation of High-Quality I?III?VI Semiconductor Nanocrystals by Tuning Relative Reactivity of Cationic Precursors. J. Am. Chem. Soc.. 131(15):5691-5697. https://doi.org/10.1021/ja9005767
38.
Miao S, Cho Y. Toward Green Optoelectronics: Environmental-Friendly Colloidal Quantum Dots Photodetectors. Front. Energy Res.. 9 https://doi.org/10.3389/fenrg.2021.666534
39.
Shu Y, Lin X, Qin H, Hu Z, Jin Y, Peng X. 2020. Quantum Dots for Display Applications. Angew Chem Int Ed. 59(50):22312-22323. https://doi.org/10.1002/anie.202004857
40.
Wu X, Ji H, Yan X, Zhong H. 2022. Industry outlook of perovskite quantum dots for display applications. Nat. Nanotechnol.. 17(8):813-816. https://doi.org/10.1038/s41565-022-01163-8
41.
Shirasaki Y, Supran GJ, Bawendi MG, Bulovi? V. 2013. Emergence of colloidal quantum-dot light-emitting technologies. Nature Photon. 7(1):13-23. https://doi.org/10.1038/nphoton.2012.328
42.
Zheng S, Chen J, Johansson EM, Zhang X. 2020. PbS Colloidal Quantum Dot Inks for Infrared Solar Cells. iScience. 23(11):101753. https://doi.org/10.1016/j.isci.2020.101753
43.
Emin S, Singh SP, Han L, Satoh N, Islam A. 2011. Colloidal quantum dot solar cells. Solar Energy. 85(6):1264-1282. https://doi.org/10.1016/j.solener.2011.02.005
44.
Carbone L, Nobile C, De Giorgi M, Sala FD, Morello G, Pompa P, Hytch M, Snoeck E, Fiore A, Franchini IR, et al. 2007. Synthesis and Micrometer-Scale Assembly of Colloidal CdSe/CdS Nanorods Prepared by a Seeded Growth Approach. Nano Lett.. 7(10):2942-2950. https://doi.org/10.1021/nl0717661
45.
Deka S, Quarta A, Lupo MG, Falqui A, Boninelli S, Giannini C, Morello G, De Giorgi M, Lanzani G, Spinella C, et al. 2009. CdSe/CdS/ZnS Double Shell Nanorods with High Photoluminescence Efficiency and Their Exploitation As Biolabeling Probes. J. Am. Chem. Soc.. 131(8):2948-2958. https://doi.org/10.1021/ja808369e
46.
Liu L, Najar A, Wang K, Du M, Liu S(. 2022. Perovskite Quantum Dots in Solar Cells. Advanced Science. 9(7):2104577. https://doi.org/10.1002/advs.202104577
47.
Chen J, Jia D, Johansson EMJ, Hagfeldt A, Zhang X. Emerging perovskite quantum dot solar cells: feasible approaches to boost performance. Energy Environ. Sci.. 14(1):224-261. https://doi.org/10.1039/d0ee02900a
48.
García de Arquer FP, Talapin DV, Klimov VI, Arakawa Y, Bayer M, Sargent EH. 2021. Semiconductor quantum dots: Technological progress and future challenges. Science. 373(6555): https://doi.org/10.1126/science.aaz8541
49.
Ding S, Hao M, Lin T, Bai Y, Wang L. 2022. Ligand engineering of perovskite quantum dots for efficient and stable solar cells. Journal of Energy Chemistry. 69626-648. https://doi.org/10.1016/j.jechem.2022.02.006
50.
You HR, Park JY, Lee DH, Kim Y, Choi J. Recent Research Progress in Surface Ligand Exchange of PbS Quantum Dots for Solar Cell Application. Applied Sciences. 10(3):975. https://doi.org/10.3390/app10030975
51.
Albaladejo?Siguan M, Baird EC, Becker?Koch D, Li Y, Rogach AL, Vaynzof Y. 2021. Stability of Quantum Dot Solar Cells: A Matter of (Life)Time. Adv. Energy Mater.. 11(12):2003457. https://doi.org/10.1002/aenm.202003457
52.
Yuan J, Hazarika A, Zhao Q, Ling X, Moot T, Ma W, Luther JM. 2020. Metal Halide Perovskites in Quantum Dot Solar Cells: Progress and Prospects. Joule. 4(6):1160-1185. https://doi.org/10.1016/j.joule.2020.04.006
53.
Ding C, Huang Y, Shen Z, Chen X. 2021. Synthesis and Bioapplications of Ag2S Quantum Dots with Near‐Infrared Fluorescence. Advanced Materials. 33(32): https://doi.org/10.1002/adma.202007768
54.
Al Mahfuz MM, Park J, Islam R, Ko D. Colloidal Ag2Se intraband quantum dots. Chem. Commun.. 59(72):10722-10736. https://doi.org/10.1039/d3cc02203j
55.
Gui R, Jin H, Wang Z, Tan L. 2015. Recent advances in synthetic methods and applications of colloidal silver chalcogenide quantum dots. Coordination Chemistry Reviews. 29691-124. https://doi.org/10.1016/j.ccr.2015.03.023