  • Effect of intraoral aging on the setting status of resin composite and glass ionomer orthodontic adhesives.

Effect of intraoral aging on the setting status of resin composite and glass ionomer orthodontic adhesives.

American journal of orthodontics and dentofacial orthopedics : official publication of the American Association of Orthodontists, its constituent societies, and the American Board of Orthodontics (2014-04-08)
Anna Iliadi, Stefan Baumgartner, Athanasios E Athanasiou, Theodore Eliades, George Eliades
要旨

The aim of this study was to assess the effect of intraoral aging on the setting status of a resin composite and a glass ionomer adhesive, relative to control specimens stored in water. Metallic brackets were bonded with resin composite orthodontic adhesive (Transbond XT; 3M Unitek, Monrovia, Calif) or a glass ionomer cement (Fuji I; GC, Tokyo, Japan) to recently extracted premolars and kept in water for 6 months. The same materials were also bonded to the premolars of orthodontic patients. After 6 months, the teeth were carefully extracted, with the brackets intact on their buccal surfaces. All teeth were embedded in epoxy resin and sectioned buccolingually. Fourier transform infrared microscopy and Raman microscopy were used for the estimation of the degree of cure in the composite and the salt yield in the glass ionomer adhesives. The control samples of the composite showed significantly lower degrees of cure than did the retrieved specimens (52.40% ± 3.21% vs 57.62% ± 1.32% by Fourier transform infrared microscopy, and 61.40% ± 2.61% vs 67.40% ± 3.44% by Raman microscopy). Raman microscopy significantly overestimated the degree of cure and failed to provide reliable information for the salt yield in the glass ionomer cement. Fourier transform infrared microscopy showed increased, but no statistically significant difference in, aluminum-carboxylate salts in the retrieved specimens. Enhanced oxidation of residual carbon-carbon bonds in the composite and slightly increased dissolution of the weaker calcium-salt phase in the glass ionomer cement were the main differences in the intraorally aged specimens in comparison with the specimens stored in water.

材料
製品番号
ブランド
製品内容

Sigma-Aldrich
活性炭, DARCO®, −100 mesh particle size, powder
Sigma-Aldrich
活性炭, powder, -100 particle size (mesh), decolorizing
Sigma-Aldrich
活性炭, DARCO®, 20-40 mesh particle size, granular
Sigma-Aldrich
活性炭Norit®, Norit® PK 1-3, from peat, steam activated, granular
Sigma-Aldrich
活性炭Norit®, Norit® SX ultra, from peat, steam activated and acid washed, highly purified, powder
Sigma-Aldrich
活性炭, untreated, granular, ≤5 mm
Sigma-Aldrich
活性炭, DARCO®, 4-12 mesh particle size, granular
Sigma-Aldrich
活性炭, DARCO®, 12-20 mesh, granular
Sigma-Aldrich
炭素, glassy, spherical powder, 2-12 μm, 99.95% trace metals basis
Supelco
活性炭, powder
Sigma-Aldrich
活性炭, acid-washed with hydrochloric acid
Sigma-Aldrich
活性炭Norit®, Norit® GAC 1240W, from coal, steam activated, granular
Sigma-Aldrich
炭素, nanopowder, <100 nm particle size (TEM)
Sigma-Aldrich
活性炭, meets USP testing specifications
Supelco
活性炭, puriss. p.a., powder
Sigma-Aldrich
活性炭Norit®, Norit® SX2, powder, from peat, multi-purpose activated charcoal, steam activated and acid washed
Sigma-Aldrich
活性炭, suitable for cell culture, suitable for plant cell culture
Sigma-Aldrich
活性炭Norit®, Norit® RB3, steam activated, rod
Sigma-Aldrich
活性炭, Norit® ROW 0.8 SUPRA, pellets
Sigma-Aldrich
活性炭, untreated, granular, 20-60 mesh
Sigma-Aldrich
活性炭, acid-washed with phosphoric and sulfuric acids
Supelco
活性炭Norit®, Norit® RBAA-3, rod
Millipore
活性炭, suitable for GC
Supelco
活性炭, for the determination of AOX, 50-150 μm particle size
Sigma-Aldrich
活性炭, SAJ first grade
炭素, foil, 10x10mm, thickness 2.0mm, hOpg
炭素, foil, 50x50mm, thickness 0.2mm, pyrolytic graphite, 99.99%
炭素, rod, 100mm, diameter 1.0mm, graphite, 99.95%
Carbon - Vitreous, rod, 100mm, diameter 5.0mm, glassy carbon
炭素, foil, 100x100mm, thickness 0.5mm, flexible graphite, 99.8%